420 deck to hulll!! |
Post Reply ![]() |
Page <12 |
Author | |
jeffers ![]() Really should get out more ![]() ![]() Joined: 29 Mar 04 Location: United Kingdom Online Status: Offline Posts: 3048 |
![]() ![]() ![]() ![]() Posted: 12 Feb 07 at 1:16pm |
I am one of the IT gurus that all schools need these days....no peace for the wicked (what did I do that was so wrong......)
|
|
Paul
---------------------- D-Zero GBR 74 |
|
![]() |
|
Garry ![]() Really should get out more ![]() ![]() Joined: 18 Apr 04 Location: United Kingdom Online Status: Offline Posts: 536 |
![]() ![]() ![]() ![]() |
Use polyester resin and filler powder NOT epoxy. All the damaged area has to be dug out back to sound glass and you will probably have to devise a method of clamping it.
And make sure you remove all the glue residue near the joint that came from the gaffer tape. Edited by Garry |
|